Analysis of Cationic Polymers
Columns: |
TSKgel G3000PWXL-CP, 7 μm, 7.8 mm ID x 30 cm
TSKgel G5000PWXL-CP, 10 μm,7.8 mm ID x 30 cm
TSKgel G6000PWXL-CP, 13 μm,7.8 mm ID x 30 cm
|
Mobile phase: |
H2O with 0.1 mol/L NaNO3 |
Flow rate: |
1 mL/min
|
Detection: |
RI |
Temperature: |
25 °C |
Sample Load: |
3 g/L, 100 μL |
|
|
Analysis of PAA
Column: |
TSKgel G5000PWXL-CP, 10 μm, 7.8 mm ID x 30 cm
|
Mobile phase: |
H2O with 0.1 mol/L NaNO3
|
Flow rate: |
1.0 mL/min |
Detection: |
RI |
Temperature: |
25 °C |
Sample: |
polyallylamine-HCl (PAA) |
Sample load: |
3 g/L, 100 μL |
|
For additional applications, please see our applications database.