Analysis of Epoxy Resin

Column: |
A. TSKgel SuperMultiporeHZ-N, 3 μm, 4.6 mm ID × 15 cm x 2
B. TSKgel SuperMultiporeHZ-M, 4 μm, 4.6 mm ID × 15 cm x 2
C. TSKgel SuperMultiporeHZ-H, 6 μm, 4.6 mm ID × 15 cm x 2
|
Mobile phase: |
THF |
|
|
Flow rate: |
0.35 mL/min |
Detection: |
UV @ 254 nm
|
Temperature: |
25 °C
|
Injection vol.: |
10 μL
|
Samples: |
epoxy resin (3 g/L) |
|
|
Analysis of Polyvinylbutyral

Column: |
TSKgel SuperMultiporeHZ-H, 6 μm,
4.6 mm ID × 15 cm × 4
|
Mobile phase: |
THF |
Flow rate: |
0.35 mL/min |
Detection: |
RI
|
Temperature: |
40 °C
|
Injection vol.: |
10 μL
|
Sample: |
polyvinylbutyral (3 g/L)
|
|
For additional applications, please see our applications database.